List of Compoflex® products
|
Product
|
Material
type
|
Weight
|
Release
coating |
Colour
|
Maximum use temperature |
Process
|
Function
|
|
|
PP
|
150 g/m2
|
None/easy release
|
White
|
|
|
Release fabric
Release film
|
|
|
PP
|
150 g/m2
|
None/easy release
|
|
|
|
Release fabric
Release film
Surface for Secondary bonding
|
Compoflex
RF 150 |
PP/PET
|
250 g/m2
|
None/easy release
|
|
|
|
Release fabric
Release film
Flow mesh
|
Compoflex
RF 3 |
PP/PET |
315 g/m2 |
None/easy release |
White/Yellow
|
* see note
|
|
Release fabric
Release film
High speed flow mesh
|
|
|
PP/PET |
250 g/m2
|
None/easy release
|
White
|
* see note
|
|
Release fabric
Release film
Flow mesh
Surface for Secondary bonding |
|
|
PP/PET |
315 g/m2
|
None/easy release |
White/Yellow
|
|
|
Release fabric
Release film
High speed flow mesh
Surface for Secondary bonding
|
Compoflex
250 |
PP |
250 g/m2 |
None/easy release |
White
|
|
Pre-preg
Wet lay up |
Release fabric
Release film
150g breather (5 oz)
|
Compoflex
SB 250 |
PP |
250 g/m2 |
None/easy release |
White
|
|
Pre-preg
Wet lay up |
Release fabric
Release film
150g breather (5 oz)
Surface for Secondary bonding
|
|
|
PP
|
400 g/m2
|
None/easy release
|
|
|
|
Release fabric
Release film
300g breather (10 oz)
|
|
|
PP
|
400 g/m2
|
None/easy release
|
|
|
|
Release fabric
Release film
300g breather (10 oz)
Surface for Secondary bonding
|
*Note: The melting point for polypropylen is 165°C (329°F) and our recommended working temperature is approx. 145°C (293°F). However,
we do have customers using Compoflex at 200°C (392°F). This is because Compoflex performs before the temperature exceeds
the melting point. Peeling is just as easy and the material becomes stable again. We recommend conducting a test on a small part
first.